BÖHLER N352S1
BÖHLER N352S1 is a martensitic chromium steel with nickel addition. Heat treatable grade, capable of taking a mirror finish. Higher corrosion resistance compared to 13% chromium steel. Resistant to the effects of seawater, weak acids and alkaline solutions, as well as to acids having a strong, oxidizing effect such as nitric acid. Surface finish for optimum corrosion resistance: fine ground or polished.
For components subject to high mechanical and corrosive stress, e.g. screws and shafts, at operating temperatures up to approx. 752° F.
Formes de produits disponibles
Produit long: ) Presented data refer exclusively to long products. Please observe the detailed explanations at the end of the data sheet (pdf).
Elaboration
Air fondu
Caractéristiques de la propriété
Acier au chrome martensitique inoxydable avec apport de Ni. Peut être trempé et revenu et apte au polissage spéculaire.
Résistant à la fois à l’eau de mer, aux solutions acides et alcalines faibles ainsi qu’aux milieux fortement oxydants comme l’acide nitrique, par exemple.
État de surface nécessaire : rectifié fin et poli.
Numéros des matériaux
- Market grade
- 431
- EN
- X15CrNi17-3
Normes
- BS
- S80
Composition chimique
* Composition chimique (% moyen)
- C
- 0.12 to 0.20
- Si
- max. 1.0
- Mn
- max. 1.0
- P
- max. 0.030
- S
- max. 0.025
- Cr
- 15 to 18.0
- Mo
- max. 0.30
- Ni
- 2.0 to 3.0
- V
- max. 0.20
- W
- max. 0.05
- Cu
- max. 0.30
- Co
- max. 0.05
- Ti
- max. 0.05
- Nb
- max. 0.05
- Fe
- REM
- Sn
- max. 0.02